Reference Source

PE Coextruded (untreated)

What is the surface energy (dyne/cm) for PE Coextruded (untreated)?

For PE Coextruded (untreated), surface energy (dyne/cm) is 30–33; condition is Fresh; needs treatment? is Yes, verified against its source on 2026-09-16.

PE Coextruded (untreated) | 30–33 | Fresh | Yes | Dyne pens | Similar to standard PE |

kolorguide.com, retrieved 2026-08-04

Material
PE Coextruded (untreated) verified
Surface energy (dyne/cm)
30–33 verified
Condition
Fresh verified
Needs treatment?
Yes verified
Sourcekolorguide.com
Verified
Review by
DatasetGalvanic series and surface energy of engineering materials