PE Coextruded (treated)
What is the surface energy (dyne/cm) for PE Coextruded (treated)?
For PE Coextruded (treated), surface energy (dyne/cm) is 38–42; condition is Corona treated; needs treatment? is No, verified against its source on 2026-09-16.
PE Coextruded (treated) | 38–42 | Corona treated | No | Dyne pens | Printable surface |
— kolorguide.com, retrieved 2026-08-04
- Material
- PE Coextruded (treated) verified
- Surface energy (dyne/cm)
- 38–42 verified
- Condition
- Corona treated verified
- Needs treatment?
- No verified