What is the surface energy (dyne/cm) for PE Coex (PA/Nylon surface)?

For PE Coex (PA/Nylon surface), surface energy (dyne/cm) is 42–50; condition is High-energy layer; needs treatment? is No, verified against its source on 2026-09-16.

PE Coex (PA/Nylon surface) | 42–50 | High-energy layer | No | Dyne pens | Excellent adhesion |

kolorguide.com, retrieved 2026-08-04

Material
PE Coex (PA/Nylon surface) verified
Surface energy (dyne/cm)
42–50 verified
Condition
High-energy layer verified
Needs treatment?
No verified