For PE Coex (EVA surface), surface energy (dyne/cm) is 36–40; condition is Modified layer; needs treatment? is Sometimes, verified against its source on 2026-08-04.

Material
PE Coex (EVA surface)
Surface energy (dyne/cm)
36–40
Condition
Modified layer
Needs treatment?
Sometimes
Sourcekolorguide.com
Verified2026-08-04
Review by2028-08-03
DatasetGalvanic series and surface energy of engineering materials

What the source says

PE Coex (EVA surface) | 36–40 | Modified layer | Sometimes | Dyne pens | Improved adhesion |