A815 · S41500
For A815 · S41500, astm specification is A815; class or grade is S41500; esab preheat group is C; esab-recommended smaw (stick) filler is OK 68.17; esab-recommended gmaw/gtaw filler is Autrod/Tigrod 410NiMo, recorded from its source on 2026-09-16.
- ASTM specification
- A815 verified
- Class or grade
- S41500 verified
- ESAB preheat group
- C verified
- ESAB-recommended SMAW (stick) filler
- OK 68.17 verified
- ESAB-recommended GMAW/GTAW filler
- Autrod/Tigrod 410NiMo verified
- ESAB-recommended SAW (submerged arc) filler
- 10.93/Autrod 410NiMo verified
- Suggested preheat, low hydrogen (H8 and less), by thickness
- T < .75: 200, .75 < T < 1.5: 300, 1.5 < T < 2.5: 300, T > 2.5: 350 our reading
- Suggested preheat, hydrogen above H8, by thickness
- T < .75: NR, .75 < T < 1.5: NR, 1.5 < T < 2.5: NR, T > 2.5: NR our reading
Values marked our reading are our classification of what the source says — the source does not print them in those words. The quote below is the evidence for each one; judge it yourself.
What the source says
A815 S31803, S32205, S32550, S32750, S32760, S32950 OK 67.55/67.53 Autrod/Tigrod 2209 TP429 C AR 309L, OK 67.13 Autrod/Tigrod 309L/309Si/310 TP430, TP430Ti C Autrod/Tigrod 430Ti/430LNb S41500 C OK 68.17 Autrod/Tigrod 410NiMo
— assets.esab.com, retrieved 2026-09-16
Where each value comes from
This source states these in separate places, so each value is shown with the passage that states it.
ESAB-recommended SAW (submerged arc) filler
10.93/Autrod 410NiMo
Suggested preheat, low hydrogen (H8 and less), by thickness and Suggested preheat, hydrogen above H8, by thickness
Preheat A B C D Low Hydrogen H8 and less T < .75 70 70 200 300 .75 < T < 1.5 70 125 300 400 1.5 < T < 2.5 150 200 300 400 T > 2.5 225 300 350 500 Hydrogen > H8 T < .75 175 175 NR NR .75 < T < 1.5 225 225 NR NR 1.5 < T < 2.5 275 275 NR NR T > 2.5 300 300 NR NR
— all from assets.esab.com, retrieved 2026-09-16
Source
- assets.esab.comhttps://assets.esab.com/assetbank-esab/assetfile/22174.pdf