Reference Source

A487 · 4E

For A487 · 4E, astm specification is A487; class or grade is 4E; esab preheat group is B; esab-recommended smaw (stick) filler is AA 12018; suggested preheat, low hydrogen (h8 and less), by thickness is T < .75: 70, .75 < T < 1.5: 125, 1.5 < T < 2.5: 200, T > 2.5: 300, recorded from its source on 2026-08-31.

ASTM specification
A487 verified
Class or grade
4E verified
ESAB preheat group
B verified
ESAB-recommended SMAW (stick) filler
AA 12018 verified
Suggested preheat, low hydrogen (H8 and less), by thickness
T < .75: 70, .75 < T < 1.5: 125, 1.5 < T < 2.5: 200, T > 2.5: 300 our reading
Suggested preheat, hydrogen above H8, by thickness
T < .75: 175, .75 < T < 1.5: 225, 1.5 < T < 2.5: 275, T > 2.5: 300 our reading
Sourceassets.esab.com
Verified
Review by
DatasetESAB recommended filler metals and suggested preheat group, by ASTM steel grade

Values marked our reading are our classification of what the source says — the source does not print them in those words. The quote below is the evidence for each one; judge it yourself.

What the source says

A487 2A, 11A, 12A, C AA 8018-NM 2B, 2C B AA 10018MM 4A, 4C, 13A B AA 9018-SR 4B, 4D B AA T 4E B AA 12018

assets.esab.com, retrieved 2026-08-31

Where each value comes from

The values above are stated away from the sentence quoted with the answer, so the passage that states them is shown here too.

Suggested preheat, low hydrogen (H8 and less), by thickness and Suggested preheat, hydrogen above H8, by thickness

Preheat A B C D Low Hydrogen H8 and less T < .75 70 70 200 300 .75 < T < 1.5 70 125 300 400 1.5 < T < 2.5 150 200 300 400 T > 2.5 225 300 350 500 Hydrogen > H8 T < .75 175 175 NR NR .75 < T < 1.5 225 225 NR NR 1.5 < T < 2.5 275 275 NR NR T > 2.5 300 300 NR NR

— all from assets.esab.com, retrieved 2026-08-31

Source

Last verified against source: . Due for re-check by . This page as Markdown · OKF bundle · full dataset as JSON.