# Any fracture or welding defect on a wheel — Vehicle inspection defect categories: MOT major, minor and dangerous verdicts For Any fracture or welding defect on a wheel, category is Dangerous; inspection item number is 5.2.2; defect reference is (a); inspection item is Road wheel condition; authority is DVSA MOT (cars, vans and passenger vehicles, classes 3, 4, 5, 7), recorded from its source on 2026-08-06. - **Defect:** Any fracture or welding defect on a wheel _(verified: appears in the quote below)_ - **Category:** Dangerous _(verified: appears in the quote below)_ - **Inspection item number:** 5.2.2 - **Defect reference:** (a) _(verified: appears in the quote below)_ - **Inspection item:** Road wheel condition - **Authority:** DVSA MOT (cars, vans and passenger vehicles, classes 3, 4, 5, 7) _(our reading, not quoted from the source)_ ## What the source says > (a) | Any fracture or welding defect on a wheel | Dangerous ## Source - https://www.gov.uk/guidance/mot-inspection-manual-for-private-passenger-and-light-commercial-vehicles/5-axles-wheels-tyres-and-suspension Last verified: 2026-08-06. Review by: 2027-02-02. Part of [Vehicle inspection defect categories: MOT major, minor and dangerous verdicts](https://referencesource.org/vehicle-inspection-defect-categories/).