# Multilayer Film (EVOH core) — Galvanic series and surface energy of engineering materials

For Multilayer Film (EVOH core), surface energy (dyne/cm) is 30–42; condition is Depends on outer layer; needs treatment? is Yes/No, verified against its source on 2026-08-04.

- **Material:** Multilayer Film (EVOH core)
- **Surface energy (dyne/cm):** 30–42
- **Condition:** Depends on outer layer
- **Needs treatment?:** Yes/No

## What the source says

> Multilayer Film (EVOH core) | 30–42 | Depends on outer layer | Yes/No | Dyne pens | Outer layer defines behavior |

## Source

- https://kolorguide.com/surface-energy-chart-by-material/

Last verified: 2026-08-04. Review by: 2028-08-03.
Part of [Galvanic series and surface energy of engineering materials](https://referencesource.org/process-compatibility-coatings-adhesives-treatments/).